Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP 7500V Russia NKNKh
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodRussia NKNKh/7500V
densityASTM D7920.9 G/cm
melt mass-flow rate230°C/2.16 kgASTM D123885-115 g/10min
Mechanical propertiesTest ConditionTest MethodRussia NKNKh/7500V
Impact strength of cantilever beam gap23℃ASTM D25640
Shore hardnessISO 86840-88 R
Flexural modulusASTM D7901200 Mpa
Thermal performanceTest ConditionTest MethodRussia NKNKh/7500V
vicatISO 306126-150
Heat distortion temperatureHDTASTM D64864-90

Contact Us

Get App

Top