EMA Optema™ TC 120 Molding ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ExxonMobil/Optema™ TC 120 Molding |
---|---|---|---|
Dart impact | -40°C | ASTM D3763 | 28.5 J |
23°C | ASTM D3763 | 17.6 J |
hardness | Test Condition | Test Method | ExxonMobil/Optema™ TC 120 Molding |
---|---|---|---|
Shore hardness | 邵氏A,15秒 | ASTM D2240 | 75 |
邵氏D,15秒 | ASTM D2240 | 28 |
Mechanical properties | Test Condition | Test Method | ExxonMobil/Optema™ TC 120 Molding |
---|---|---|---|
elongation | 断裂 | ASTM D638 | >800 % |
tensile strength | 断裂 | ASTM D638 | 5.86 MPa |
Flexural modulus | ASTM D790 | 32.8 MPa |
physical property | Test Condition | Test Method | ExxonMobil/Optema™ TC 120 Molding |
---|---|---|---|
Methacrylic acid content | ExxonMobilMethod | 21.5 wt% | |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 6.0 g/10min |
Thermal performance | Test Condition | Test Method | ExxonMobil/Optema™ TC 120 Molding |
---|---|---|---|
vicat | ASTM D1525 | 48.0 °C |