Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| aging | Test Condition | Test Method | SHANDONG DAWN/10-55A |
|---|---|---|---|
| Change rate of ultimate elongation in air | 720 hr | ASTM D573 | 9.0 % |
| Change rate of tensile strength in air | 720 hr | ASTM D573 | 3.0 % |
| Change rate of tensile modulus in air | 720 hr | ASTM D573 | 3.0 % |
| Volume change | 70 hr, ASTM 标准油(3号) | IEC 6093 | 20 % |
| mechanical properties | Test Condition | Test Method | SHANDONG DAWN/10-55A |
| tear strength | ASTM D-624 | 16.6 kN/m | |
| elongation | Break | ASTM D-412 | 460 % |
| Tensile modulus | ASTM D-412 | 1.70 Mpa | |
| Permanent compression deformation | 100°C, 168 hr | ASTM D-395 | 21 % |
| tensile strength | Yield | ASTM D-412 | 5.50 MP |
| Physical properties | Test Condition | Test Method | SHANDONG DAWN/10-55A |
| Shore hardness | Shore A, 5 Sec | ASTM D-2240 | 55 |
| thermal performance | Test Condition | Test Method | SHANDONG DAWN/10-55A |
| Continuous use temperature | -60.0 - 135 °C |