Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPV 10-55A SHANDONG DAWN
--
Application in the automotive field,Consumer product application field,Electrical/Electronic Applications,Architectural application field
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SHANDONG DAWN/10-55A |
|---|---|---|---|
| Continuous use temperature | -60.0 - 135 °C |
| mechanical properties | Test Condition | Test Method | SHANDONG DAWN/10-55A |
|---|---|---|---|
| elongation | Break | ASTM D-412 | 460 % |
| Permanent compression deformation | 100°C, 168 hr | ASTM D-395 | 21 % |
| tear strength | ASTM D-624 | 16.6 kN/m | |
| Tensile modulus | ASTM D-412 | 1.70 Mpa | |
| tensile strength | Yield | ASTM D-412 | 5.50 MP |
| Physical properties | Test Condition | Test Method | SHANDONG DAWN/10-55A |
|---|---|---|---|
| Shore hardness | Shore A, 5 Sec | ASTM D-2240 | 55 |
| aging | Test Condition | Test Method | SHANDONG DAWN/10-55A |
|---|---|---|---|
| Change rate of tensile modulus in air | 720 hr | ASTM D573 | 3.0 % |
| Change rate of tensile strength in air | 720 hr | ASTM D573 | 3.0 % |
| Change rate of ultimate elongation in air | 720 hr | ASTM D573 | 9.0 % |
| Volume change | 70 hr, ASTM 标准油(3号) | IEC 6093 | 20 % |