PP PPU0180F EXXONMOBIL USA
ExxonMobil™
--
High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | EXXONMOBIL USA/PPU0180F |
|---|---|---|---|
| Hot deformation temperature | 1.80MPaAnnealed | ISO 75-2/Af | 53.9 °C |
| mechanical properties | Test Condition | Test Method | EXXONMOBIL USA/PPU0180F |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 1.99 kJ/m² |
| Tensile modulus | 23°C | ISO 527-2 | 1500 Mpa |
| Physical properties | Test Condition | Test Method | EXXONMOBIL USA/PPU0180F |
|---|---|---|---|
| melt mass-flow rate | 230℃/2.16Kg | ISO 1133 | 10 g/10min |
| 比重 | ASTM D-256-97 | 0.9 g/cm³ |