Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ABS 250 TORAY JAPAN
Toyolac®
Industrial machinery,Fitness equipment
High mobility,High rigidity
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| Rockwell hardness | R-Sale,23°C | ASTM D785 | 115 |
| R-Sale,23°C | ISO 2039-2 | 115 |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 83.0 °C |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 87.0 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7E-05 cm/cm/°C |
| Vicat softening temperature | 95.0 °C |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 2580 Mpa |
| ASTM D790 | 2550 Mpa | ||
| bending strength | 23°C | ISO 178 | 83.0 Mpa |
| ASTM D790 | 77.0 Mpa | ||
| elongation | Break | ASTM D638 | 20 % |
| Tensile strain | Break,23°C | ISO 527-2 | 16 % |
| tensile strength | ASTM D638 | 51.0 Mpa | |
| Yield,23°C | ISO 527-2 | 57.0 Mpa |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| density | 23°C | ISO 1183 | 1.05 g/cm³ |
| ASTM D792 | 1.05 g/cm³ | ||
| melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 48 g/10min |
| Shrinkage rate | Internal Method | 0.40-0.60 % |
| impact performance | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 10 kJ/m² |
| Impact strength of cantilever beam gap | -30°C,3.20mm | ASTM D256 | 69 J/m |
| -30°C,12.7mm | ASTM D256 | 69 J/m | |
| 23°C,12.7mm | ASTM D256 | 110 J/m | |
| 0°C,12.7mm | ASTM D256 | 78 J/m | |
| 23°C,3.20mm | ASTM D256 | 170 J/m | |
| 0°C,3.20mm | ASTM D256 | 88 J/m |
| flammability | Test Condition | Test Method | TORAY JAPAN/250 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |