Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM M270 FPC TAIWAN
FORMOCON®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | FPC TAIWAN/M270 |
---|---|---|---|
Combustibility (rate) | UL 94 | HB | |
Hot deformation temperature | HDT | ASTM D648/ISO 75 | 158 ℃(℉) |
Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 8.45 mm/mm.℃ | |
Melting temperature | 165 ℃(℉) | ||
Vicat softening temperature | ASTM D1525/ISO R306 | 162 ℃(℉) |
mechanical properties | Test Condition | Test Method | FPC TAIWAN/M270 |
---|---|---|---|
Bending modulus | ASTM D790/ISO 178 | 26000 kg/cm²(MPa)[Lb/in²] | |
bending strength | ASTM D790/ISO 178 | 950 kg/cm²(MPa)[Lb/in²] | |
Elongation at Break | ASTM D638/ISO 527 | 45 % | |
Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 5.4 kg·cm/cm(J/M)ft·lb/in | |
Rockwell hardness | ASTM D785 | 80 |
Electrical performance | Test Condition | Test Method | FPC TAIWAN/M270 |
---|---|---|---|
Surface resistivity | ASTM D257/IEC 60093 | 1E+16 Ω | |
Volume resistivity | ASTM D257/IEC 60093 | 1E+14 Ω.cm |
other | Test Condition | Test Method | FPC TAIWAN/M270 |
---|---|---|---|
characteristic | 高流动性、 | ||
purpose | 细微型 |
Physical properties | Test Condition | Test Method | FPC TAIWAN/M270 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.41 | |
Shrinkage rate | ASTM D955 | 1.8-2.2 % | |
Water absorption rate | ASTM D570/ISO 62 | 0.22 % |