PET CB-606 Far Spinning Shanghai
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodFar Spinning Shanghai/CB-606
acid valueMaX.35 Meq/Kg
Acetaldehyde contentGB 17931≤1.0 PPm
ash content0.01-0.05 %
Fixed viscosityASTM D-46030.840±0.020 dl/g
melting temperatureDSC247±2
colour and lustreL(Lb)COLORQUESTXE87.0±2(-1.5±1.0)