| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/KL-4010 GY |
|---|---|---|---|
| elongation | Break | ASTM D638 | 34 % |
| bending strength | ISO 178 | 70.0 Mpa | |
| Tensile strain | Break | ISO 527-2 | 30 % |
| tensile strength | Break | ISO 527-2 | 53.0 Mpa |
| Tensile modulus | ISO 527-2/1 | 2620 Mpa | |
| ASTM D638 | 2760 Mpa | ||
| bending strength | ASTM D790 | 13.8 Mpa | |
| Friction coefficient | Static | ASTM D3702Modified | 0.18 |
| Tensile strain | Yield | ISO 527-2 | 11 % |
| Wear factor | Washer | ASTM D3702Modified | 22.5 10^-10in^5-min/ft-lb-hr |
| tensile strength | Break | ASTM D638 | 52.4 Mpa |
| Yield | ASTM D638 | 55.2 Mpa | |
| Yield | ISO 527-2 | 54.0 Mpa | |
| Bending modulus | ASTM D790 | 3450 Mpa | |
| ISO 178 | 2000 Mpa | ||
| elongation | Yield | ASTM D638 | 9.9 % |
| Friction coefficient | Dynamic | ASTM D3702Modified | 0.38 |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/KL-4010 GY |
| Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 96.0 °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 112 °C | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ISO 11359-2 | 1.2E-04 cm/cm/°C |
| MD:-40to40°C | ASTME831 | 1.2E-04 cm/cm/°C | |
| TD:-40to40°C | ASTME831 | 1.1E-04 cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO 75-2/Bf | 149 °C |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 158 °C | |
| Linear coefficient of thermal expansion | TD:-40to40°C | ISO 11359-2 | 1.1E-04 cm/cm/°C |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/KL-4010 GY |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 48 kJ/m² |
| Multi axis Instrumented Impact Energy | ISO 6603-2 | 0.900 J | |
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 5.30 J |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 1000 kJ/m² |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/KL-4010 GY |
| Shrinkage rate | MD:24hr | ASTM D955 | 2.3 % |
| MD:24hr | ISO 294-4 | 2.3 % | |
| TD:24hr | ASTM D955 | 2.3 % | |
| TD:24hr | ISO 294-4 | 2.3 % | |
| Water absorption rate | 24hr,50%RH | ASTM D570 | 0.20 % |