plas

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC/PET UT250 COVESTRO GERMANY
Makroblend® 
Electronic field,Electrical field
High mobility,Dimensional stability,High temperature resistan
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodCOVESTRO GERMANY/UT250
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B125 °C
1.8MPa,UnannealedISO 75-2/A110 °C
Vicat softening temperatureISO 306/B120140 °C
mechanical propertiesTest ConditionTest MethodCOVESTRO GERMANY/UT250
Nominal tensile fracture strain23°CISO 527-2/50>50 %
Tensile modulus23°CISO 527-2/12250 Mpa
Tensile strainYield,23°CISO 527-2/505.0 %
tensile strengthBreak,23°CISO 527-2/5050.0 Mpa
Yield,23°CISO 527-2/5055.0 Mpa
Physical propertiesTest ConditionTest MethodCOVESTRO GERMANY/UT250
Melt Volume Flow Rate (MVR)265°C/5.0kgISO 113322.0 cm3/10min
Shrinkage rateTD2ISO 25770.60-0.80 %
TD:90°C,1hrISO 25770.10-0.20 %
MD2ISO 25770.60-0.80 %
MD:90°C,1hrISO 25770.10-0.20 %
impact performanceTest ConditionTest MethodCOVESTRO GERMANY/UT250
Impact strength of cantilever beam gap-20°CISO 180/A40 kJ/m²
23°CISO 180/1CNoBreak
23°CISO 180/A50 kJ/m²
-30°CISO 180/1CNoBreak