Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | LYONDELLBASELL SAUDI/HP462R |
|---|---|---|---|
| tensile strength | Yield | ISO 527-1 | 34 Mpa |
| Bending modulus | ISO 178 | 1450 Mpa | |
| Tensile strain | Yield | ISO 527-1 | 8 % |
| Break | ISO 527-1 | 50 % | |
| Basic Performance | Test Condition | Test Method | LYONDELLBASELL SAUDI/HP462R |
| Melt Volume Flow Rate (MVR) | 230°C/2.16 kg | ISO 1133 | 34 CM |
| thermal performance | Test Condition | Test Method | LYONDELLBASELL SAUDI/HP462R |
| Vicat softening temperature | B50 (50°C/h 10N) | ISO 306 | 90 °C |
| A50 (50°C/h 10N) | ISO 306 | 154 °C | |
| Hot deformation temperature | 0.45Mpa, Unannealed | ISO 75B-1 | 85 °C |