Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP-R R200P HYOSUNG KOREA
TOPILENE®
Building water supply system,Floor heating system,Radiator heating,Chemical tubing,Agricultural pipe,Pipe fittings
High temperature resistan,High voltage resistance,Chemical stability perfor,Heat resistance,high strength
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | HYOSUNG KOREA/R200P |
|---|---|---|---|
| density | ASTM D792 | 0.91 g/cm³ | |
| melt mass-flow rate | 230℃,2.16kg | ASTM D-1238 | 0.2 g/10min |
| 190℃,5.0kg | ASTM D-1238 | 0.4 g/10min |
| thermal performance | Test Condition | Test Method | HYOSUNG KOREA/R200P |
|---|---|---|---|
| Linear coefficient of thermal expansion | 0-110℃ | Dilatometer | 1.5×10-4 |
| Melting temperature | HS Method | 141 °C | |
| 141 ℃(℉) | |||
| Vicat softening temperature | ASTM D-1525 | 130 °C | |
| ASTM D1525/ISO R306 | 130 ℃(℉) |
| mechanical properties | Test Condition | Test Method | HYOSUNG KOREA/R200P |
|---|---|---|---|
| Bending modulus | ASTM D-790 | 8.500 kg/cm2 | |
| ASTM D790/ISO 178 | 9000 % | ||
| elongation | ASTM D-638 | >400 % | |
| Elongation at Break | ASTM D638/ISO 527 | >400 kg/cm²(MPa)[Lb/in²] | |
| Impact strength of cantilever beam gap | 0℃ | ASTM D-256 | 8 kg·cm/cm |
| 23℃ | ASTM D-256 | No break kg·cm/cm | |
| -20℃ | ASTM D-256 | 3 kg·cm/cm | |
| Rockwell hardness | ASTM D785 | 75 | |
| tensile strength | ASTM D638/ISO 527 | 270 kg/cm²(MPa)[Lb/in²] | |
| 降伏点 | ASTM D-638 | 270 kg/cm2 | |
| 破断点 | ASTM D-638 | 230 kg/cm2 | |
| Volume resistivity | HS Method | >1013 Ω |
| Physical properties | Test Condition | Test Method | HYOSUNG KOREA/R200P |
|---|---|---|---|
| density | ASTM D792/ISO 1183 | 0.91 | |
| melt mass-flow rate | ASTM D1238/ISO 1133 | 0.25 g/10min |