PP H030 GP SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SIBUR RUSSIA/H030 GP |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | Internal Method | 80.0 °C |
Vicat softening temperature | Internal Method4 | 155 °C |
mechanical properties | Test Condition | Test Method | SIBUR RUSSIA/H030 GP |
---|---|---|---|
Bending modulus | Internal Method | 1500 Mpa | |
Tensile strain | Yield | Internal Method | 10 % |
tensile strength | Yield | Internal Method | 30.0 Mpa |
Physical properties | Test Condition | Test Method | SIBUR RUSSIA/H030 GP |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | Internal Method | 3.0 g/10min |
impact performance | Test Condition | Test Method | SIBUR RUSSIA/H030 GP |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | Internal Method | 2.0 kJ/m² |