Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPA HTN54G35HSLR BK031 DUPONT JAPAN
Zytel®
Electronic and Electrical Applications
Thermal stability,enhance,Filler: Glass fiber reinf,35% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DUPONT JAPAN/HTN54G35HSLR BK031 |
|---|---|---|---|
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 6E-05 cm/cm/°C |
| MD | ISO 11359-2 | 2E-05 cm/cm/°C | |
| Vicat softening temperature | Melting Temperature | ISO 11357-3 | 300 °C |
| mechanical properties | Test Condition | Test Method | DUPONT JAPAN/HTN54G35HSLR BK031 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 11 kJ/m² |
| Elongation at Break | 23°C | ISO 527-2 | 2.70 % |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 82 kJ/m² |
| Tensile modulus | 23°C | ISO 527-2 | 10500 Mpa |
| tensile strength | 23°C | ISO 527-2 | 185 Mpa |
| Electrical performance | Test Condition | Test Method | DUPONT JAPAN/HTN54G35HSLR BK031 |
|---|---|---|---|
| Dielectric strength | 0.250mm | IEC 60243-1 | 33 KV/mm |
| Dissipation factor | 相对漏电起痕指数 | IEC 60112 | 575 V |
| Volume resistivity | IEC 60093 | >1.0E+15 Ω.cm |
| Physical properties | Test Condition | Test Method | DUPONT JAPAN/HTN54G35HSLR BK031 |
|---|---|---|---|
| Shrinkage rate | TD2.0mm | ISO 294-4 | 0.50 % |
| MD2.0mm | ISO 294-4 | 0.20 % |