Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 7022IRF MITSUBISHI ENGINEERING JAPAN
IUPILON™
--
Low viscosity、Easy to demould
FDA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022IRF |
---|---|---|---|
Flame retardancy | 1.6mm | UL 94 | V-2 |
Heat Deflection Temperature | 0.455KPa | ASTM D-648 | 145 °C |
Mechanical Properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022IRF |
---|---|---|---|
Flexural Modulus | 23℃ | ASTM D-790 | 2.3 GPa |
Tensile Strength | 23℃ | ASTM D-638 | 60.8 Mpa |
Flexural Strength | 23℃ | ASTM D-790 | 88.2 Mpa |
Tensile Elongation?(Break) | 23℃ | ASTM D-638 | 110 % |
IZOD Notch Impact Strength | 3.2mm | ASTM D-256 | 880 J/m |
Rockwell Hardness | ASTM D-785 | R120 |
Physical | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022IRF |
---|---|---|---|
Moisture Absorption | 23℃,24时间 | ASTM D-570 | 0.15 % |
Electrical Properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022IRF |
---|---|---|---|
Dielectric Strength | ASTM D-149 | 16 MV/m | |
Dissipation Factor? | 106Hz | ASTM D-150 | 0.0092 |
Dielectric Constant | 106Hz | ASTM D-150 | 25.2 Pf/m |
Surface Resistivity | ASTM D-257 | >1015 Ohm | |
Volume Resistivity | ASTM D-257 | 4-016 ohm-cm |