Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

GPPS HSF 13 N Schulman Plastics
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | Schulman Plastics/HSF 13 N |
|---|---|---|---|
| density | ISO 1183 | 1.21 | |
| Melt Volume Flow Rate (MVR) | 200℃,5kg | ISO 1133 | 7.00 cm |
| thermal performance | Test Condition | Test Method | Schulman Plastics/HSF 13 N |
|---|---|---|---|
| Combustibility | 3.00mm | UL 94 | V-0 |
| 1.50mm | UL 94 | V-0 | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75B-1 | 84.0 ℃ |
| 1.80MPa,Unannealed | ISO 75A-1 | 72.0 ℃ | |
| Limiting Oxygen Index (LOI) | ISO 4589-1-2 | 24 % | |
| Vicat softening temperature | B50(50N,50℃/h) | ISO 306 | 85.0 ℃ |
| A50(50N,50℃/h) | ISO 306 | 95.0 ℃ |
| mechanical properties | Test Condition | Test Method | Schulman Plastics/HSF 13 N |
|---|---|---|---|
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 7.00 KJ/m |
| -30℃ | ISO 179/1eA | 5.00 KJ/m | |
| Impact strength of simply supported beam without notch | 23℃ | ISO 179/1eU | 50.0 KJ/m |
| -30℃ | ISO 179/1eU | 39.0 KJ/m | |
| Shore hardness | ISO 2039-1 | 96.0 MPa | |
| Tensile modulus | ISO 527-1 | 2100 MPa | |
| Tensile strain | Yield | ISO 527-1 | 2.0 % |
| Tensile stress | Yield | ISO 527-1 | 27.0 MPa |