EAA 5050 EXXONMOBIL USA
ESCOR™
chip,container
Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | EXXONMOBIL USA/5050 |
---|---|---|---|
density | ASTM D-4703/D-1505 | 0.936 g/m3 | |
melt mass-flow rate | ASTM D-1238 | 8.4 g/10min |
thermal performance | Test Condition | Test Method | EXXONMOBIL USA/5050 |
---|---|---|---|
Maximum melting temperature | ASTM D-3418 | 97 °C | |
Vicat softening temperature | ASTM D-1525 | 77 °C |
Physical properties | Test Condition | Test Method | EXXONMOBIL USA/5050 |
---|---|---|---|
Acrylic acid content | ExxonMobil Method | 9 %wt |