Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP AW191 TPC SINGAPORE
COSMOPLENE®
Industrial applications,Automotive sector,Loading box
High impact resistance,Impact copolymer,Middle flow
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 68 |
| thermal performance | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 110 °C |
| mechanical properties | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 870 Mpa | |
| elongation | Break | ASTM D638 | 500 % |
| tensile strength | Yield | ASTM D638 | 20.0 Mpa |
| Break | ASTM D638 | 22.5 Mpa |
| Physical properties | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| density | ASTM D792 | 0.900 g/cm³ | |
| melt mass-flow rate | ASTM D1238 | 10 g/10min | |
| Shrinkage rate | MD:2.00mm | Internal Method | 1.4 % |
| TD:2.00mm | Internal Method | 1.4 % |
| impact performance | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| Impact strength of cantilever beam gap | -20°C | ASTM D256 | 80 J/m |
| 23°C | ASTM D256 | 550 J/m |
| flammability | Test Condition | Test Method | TPC SINGAPORE/AW191 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |