Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | TECHMER PM US/J-4/35/TF/15 |
|---|---|---|---|
| elongation | Break | ASTM D638 | 3.0 % |
| tensile strength | ASTM D638 | 138 Mpa | |
| bending strength | ASTM D790 | 214 Mpa | |
| compressive strength | ASTM D695 | 131 Mpa | |
| Bending modulus | ASTM D790 | 8340 Mpa | |
| thermal performance | Test Condition | Test Method | TECHMER PM US/J-4/35/TF/15 |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 4.9E-5 cm/cm/°C |
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 199 °C |
| Physical properties | Test Condition | Test Method | TECHMER PM US/J-4/35/TF/15 |
| Water absorption rate | 24 hr | ASTM D570 | 0.13 % |
| Shrinkage rate | 3.18 mm,Flow | ASTM D955 | 0.20 % |
| hardness | Test Condition | Test Method | TECHMER PM US/J-4/35/TF/15 |
| Rockwell hardness | R-Scale | ASTM D785 | 117 |
| flammability | Test Condition | Test Method | TECHMER PM US/J-4/35/TF/15 |
| UL flame retardant rating | 1.6 mm | UL 94 | HB |