ABS Romiloy® 4010/02 UV GF8 ROMIRA GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/02 UV GF8 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 10 kJ/m² |
-30°C | ISO 179/1eA | 5.0 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 45 kJ/m² |
-30°C | ISO 179/1eU | 40 kJ/m² |
Mechanical properties | Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/02 UV GF8 |
---|---|---|---|
Tensile strain | 断裂,23°C | ISO 527-2/5 | >30 % |
tensile strength | 23°C | ISO 527-2/5 | 43.0 MPa |
Flexural modulus | 23°C | ISO 178 | 2550 MPa |
Tensile modulus | 23°C | ISO 527-2/1 | 2500 MPa |
bending strength | 23°C | ISO 178 | 66.0 MPa |
flammability | Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/02 UV GF8 |
---|---|---|---|
UL flame retardant rating | 1.6mm | UL 94 | HB |
physical property | Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/02 UV GF8 |
---|---|---|---|
Shrinkage rate | 23°C | ISO 294-4 | 0.30to0.70 % |
density | 23°C | ISO 1183 | 1.12 g/cm³ |
melt mass-flow rate | 260°C/5.0kg | ISO 1133 | 16 g/10min |
Thermal performance | Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/02 UV GF8 |
---|---|---|---|
vicat | ISO 306/B50 | 126 °C |