Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP HP562T LYONDELLBASELL HOLAND
Moplen
spunbond 、Textile application
Excellent deep drawing an、Molecular weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP562T |
---|---|---|---|
density | ASTM D1505 | 0.9 g/cm | |
melt mass-flow rate | MFR | ASTM D1238 | 60 g/10min |
Mechanical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP562T |
---|---|---|---|
tensile strength | Yield | ASTM D638 | 37.3 Mpa |
elongation | Yield | ASTM D638 | 8 % |
Shore hardness | ASTM D785 | 98 | |
Impact strength of cantilever beam gap | 23℃ | ASTM D256 | 24.5 |
Flexural modulus | ASTM D790 | 1470 Mpa |
Thermal performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP562T |
---|---|---|---|
Heat distortion temperature | 0.45Mpa, Unannealed,HDT | ASTM D648 | 100 °C |
Contact Us
Get App
Top