Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ASA 776SE BK BASF GERMANY
Luran®S
--
Good strength
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
Rockwell hardness | R -Sale | ASTM D785 | 89 |
thermal performance | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 83.0 °C |
0.45 MPa, Unannealed | ASTM D648 | 101 °C | |
Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 0.000095 cm/cm/℃ |
Vicat softening temperature | ASTM D15253 | 92.0 °C |
mechanical properties | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
Bending modulus | 23℃ | ASTM D790 | 1660 Mpa |
bending strength | 23℃ | ASTM D790 | 47.0 Mpa |
Charpy Notched Impact Strength | -40℃ | ASTM D256 | 51 J/m |
23℃ | ASTM D256 | 260 J/m | |
elongation | Yield, 23℃ | ASTM D638 | 2.7 % |
Tensile modulus | 23℃ | ASTM D638 | 1650 Mpa |
tensile strength | Yield, 23℃ | ASTM D638 | 33.0 |
Electrical performance | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
Compared to the anti leakage trace index | IEC 60112 | V | |
Dielectric constant | 1.00 mm, 1 MHz | ASTM D150 | 3.40 |
1 MHz | IEC 60250 | 3.40 | |
100 Hz | IEC 60250 | 3.80 | |
Dielectric strength | IEC 60243-1 | 35 KV/mm | |
Dissipation factor | 100 Hz | IEC 60250 | 0.0090 |
1 MHz | IEC 60250 | 0.034 | |
Surface resistivity | ASTM D257 | >1.0E+13 Ohm | |
Volume resistivity | ASTM D257 | >1.0E+14 ohm·cm |
other | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
gloss | 60° | ASTM D523 | 48 |
Physical properties | Test Condition | Test Method | BASF GERMANY/776SE BK |
---|---|---|---|
Melt Volume Flow Rate (MVR) | MVR 220°C/10.0 kg | ASTM D1238 | 4.00 cm3/10min |
Shrinkage rate | MD | ASTM D955 | 0.55 % |
Water absorption rate | Saturation, 23℃ | ASTM D570 | 1.7 % |