LDPE LDPE LD 419.MV ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | ExxonMobil/LDPE LD 419.MV |
---|---|---|---|
Shore hardness | 邵氏A,15秒 | ASTM D2240 | 90 |
邵氏D,15秒 | ASTM D2240 | 44 |
Electrical performance | Test Condition | Test Method | ExxonMobil/LDPE LD 419.MV |
---|---|---|---|
Volume resistivity | ASTM D257 | 7.6E+15 ohms·cm | |
Dissipation Factor | ASTM D150 | 7.5E-05 | |
dielectric strength | ASTM D149 | 50 kV/mm | |
dielectric constant | ASTM D150 | 2.29 |
Mechanical properties | Test Condition | Test Method | ExxonMobil/LDPE LD 419.MV |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 630 % |
屈服 | ASTM D638 | 14 % | |
tensile strength | 断裂 | ASTM D638 | 10.3 MPa |
Flexural modulus | ASTM D790 | 243 MPa | |
tensile strength | 屈服 | ASTM D638 | 11.6 MPa |
physical property | Test Condition | Test Method | ExxonMobil/LDPE LD 419.MV |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 2.3 g/10min |