ABS TAIRILAC® AG15E1 FORMOSA NINGBO
1039
- Unit Price:
- $1585 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 918.9MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High gloss High gloss High impact resistance
- Application Areas:Electrical field Electronic field
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density / Specific Gravity | 23℃/23℃ | ASTM D-792(ISO 1183) | 1.05 |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | 23℃ | ASTM D-638(ISO 527) | 530(52) | kg/cm2(MPa) |
Flexural Strength | 23℃ | ASTM D-790(ISO 178) | 870(86) | kg/cm2(MPa) |
flexural modulus | 23℃ | ASTM D-790(ISO 178) | 28000(2750) | kg/cm2(MPa) |
Rockwell Hardness | 23℃ | ASTM D-785(ISO 2039/2) | R-110 | |
Izod Impact Strength | 23℃ | ASTM D-256(ISO R180) | 14(137) | kg.cm/cm(J/m) |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | Unannealed 18.6kg/cm2 (1/2"厚) | ASTM D-648(ISO 75/A) | 88 | °C |
Annealed (8℃×8hr) | ASTM D-648(ISO 75/A) | 100 | °C | |
Vicat Softening Temperature | 1Kg load | ASTM D-1525(ISO 306) | 103 | °C |
Flammability | FILE NO E162823 | UL 94 | 1/16"HB All Color |
Physical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt index | 220℃×10kgf(98N) | ASTM D-1238(ISO 1133) | 20 | g/10min |
200℃×5kgf(49N) | ASTM D-1238(ISO 1133) | 1.8 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.