Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Mass-Flow Rate | 190°C/21.6kg | ASTMD1238 | 1.4 | g/10min |
Melt Mass-Flow Rate | 190°C/2.16kg | ISO1133 | 1.3 | g/10min |
Viscosity number | | ISO307 | 600 | cm³/g |
Solid Content | | ISO1628-3 | 6.0 | dl/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strain | Yield | ISO527-2/1A/50 | 9.0 | % |
Nominal Tensile Strain at Break | | ISO527-2/1A/50 | >50 | % |
Tensile Creep Modulus | 1hr | ISO899-1 | 680 | Mpa |
Tensile Creep Modulus | 1000hr | ISO899-1 | 340 | Mpa |
WearbySandslurryMethod3 | | 内部方法 | 310 | |
Abrasion Loss | | 内部方法 | 250 | |
Tensile Modulus | | ISO527-2/1A/1 | 1100 | Mpa |
Tensile Stress | Yield | ISO527-2/1A/50 | 26.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD | ASTMD696,ISO11359-2 | 2E-04 | cm/cm/°C |
Specific Heat | 23°C | 内部方法 | 1840 | J/kg/°C |
Thermal Conductivity | 23°C | 内部方法 | 0.41 | W/m/K |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 75.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 41.0 | °C |
Vicat Softening Temperature | | ASTMD1525,ISO306/B50 | 80.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | -- | ASTMD257 | >1.0E+13 | ohms |
Surface Resistivity | -- | IEC60093 | >1.0E+12 | ohms |
Volume Resistivity | -- | ASTMD257 | >1.0E+15 | ohms·cm |
Volume Resistivity | -- | IEC60093 | >1.0E+14 | ohms·cm |
Dielectric Strength | | IEC60243-1 | 40 | KV/mm |
Dielectric Constant | 1MHz | ASTMD150 | 2.90 | |
Dielectric Constant | 100Hz | IEC60250 | 2.00 | |
Dielectric Constant | 1MHz | IEC60250 | 2.00 | |
Dissipation Factor? | 100Hz | IEC60250 | 2E-04 | |
Dissipation Factor? | 1MHz | IEC60250 | 4E-04 | |
Comparative Tracking Index | | IEC60112 | 600 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Notched Impact Strength | | ISO1152-2 | 25.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore D | ASTMD2240 | 63 | |
Shore Hardness | Shore D,15sec | ISO868 | 63 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.6mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.