PC LEXAN™ EXL9330 GY4D167 SABIC INNOVATIVE SINGAPHORE
2
- Unit Price:US$ 4,300 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Dongguan Zhengxingyuan Plastics Co., Ltd.
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|Toughening|UV resistance
- Application Areas:Casters|Thin walled products|food
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 800 | J/m |
| -30°C10 | ISO 180/4A | 65 | kJ/m² | |
| -30°C9 | ISO 180/1A | 55 | kJ/m² | |
| 23°C9 | ISO 180/1A | 70 | kJ/m² | |
| 23°C10 | ISO 180/4A | 80 | kJ/m² | |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | 无断裂 | |
| 23°C | ISO 180/1U | 无断裂 | ||
| Dart impact | 23°C, Total Energy | ASTM D3763 | 52.0 | J |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 60 | kJ/m² |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 75 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 无断裂 | |
| Impact strength of cantilever beam gap | -30°C | ASTM D256 | 680 | J/m |
| -50°C | ASTM D256 | 590 | J/m | |
| 23°C, 6.40 mm | ASTM D256 | 640 | J/m | |
| 23°C8 | Internal Method | 1100 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 3.0 mm | UL 94 | 5VA | |
| 1.5 mm | UL 94 | V-0 | ||
| Hot filament ignition temperature | 1.0 mm | IEC 60695-2-13 | 825 | °C |
| Burning wire flammability index | 1.0 mm | IEC 60695-2-12 | 960 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 35 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | --5,6 | ISO 178 | 85.0 | Mpa |
| Yield, 50.0 mm Span4 | ASTM D790 | 88.0 | Mpa | |
| Bending modulus | --5 | ISO 178 | 2200 | Mpa |
| 50.0 mm Span4 | ASTM D790 | 2060 | Mpa | |
| tensile strength | Yield3 | ASTM D638 | 58.0 | Mpa |
| Tensile modulus | -- | ISO 527-2/1 | 2100 | Mpa |
| --2 | ASTM D638 | 2100 | Mpa | |
| elongation | Break | ISO 527-2/50 | 130 | % |
| Break3 | ASTM D638 | 130 | % | |
| Yield | ISO 527-2/50 | 6.0 | % | |
| tensile strength | Break | ISO 527-2/50 | 60.0 | Mpa |
| elongation | Yield3 | ASTM D638 | 6.0 | % |
| tensile strength | Break3 | ASTM D638 | 61.0 | Mpa |
| Yield | ISO 527-2/50 | 55.0 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Mold temperature | 70 to 95 | °C | ||
| Processing (melt) temperature | 295 to 315 | °C | ||
| Spray nozzle temperature | 290 to 310 | °C | ||
| Temperature at the front of the material cylinder | 295 to 315 | °C | ||
| Temperature in the middle of the barrel | 280 to 305 | °C | ||
| Temperature at the rear of the barrel | 215 to 295 | °C | ||
| Suggested injection volume | 40 to 60 | % | ||
| Suggested maximum moisture content | 0.020 | % | ||
| drying time | 3.0 to 4.0 | hr | ||
| drying temperature | 120 | °C | ||
| Exhaust hole depth | 0.025 to 0.076 | mm | ||
| Screw speed | 40 to 70 | rpm | ||
| Back pressure | 0.300 to 0.700 | Mpa | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| RTI Imp | UL 746 | 115 | °C | |
| RTI | UL 746 | 120 | °C | |
| Hot deformation temperature | 0.45 MPa, Unannealed, 3.20 mm | ASTM D648 | 134 | °C |
| RTI Elec | UL 746 | 125 | °C | |
| Linear coefficient of thermal expansion | Across Flow : 23 to 80°C | ISO 11359-2 | 7.7E-5 | cm/cm/°C |
| Across Flow : -40 to 40°C | ASTM E831 | 6.7E-5 | cm/cm/°C | |
| Flow : 23 to 80°C | ISO 11359-2 | 7.2E-5 | cm/cm/°C | |
| Flow : -40 to 40°C | ASTM E831 | 6.7E-5 | cm/cm/°C | |
| Ball Pressure Test | 123 to 127°C | IEC 60695-10-2 | 通过 | |
| Vicat softening temperature | -- | ISO 306/B50 | 140 | °C |
| -- | ASTM D152512 | 142 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm, 100 mm Span11 | ISO 75-2/Ae | 124 | °C |
| 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 124 | °C | |
| 1.8 MPa, Unannealed, 3.20 mm | ASTM D648 | 120 | °C | |
| 0.45 MPa, Unannealed, 4.00 mm, 100 mm Span11 | ISO 75-2/Be | 135 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | Across FlowFlow : 3.20 mm | Internal Method | 0.40 - 0.80 | % |
| Flow : 3.20 mm | Internal Method | 0.40 - 0.80 | % | |
| Melt Volume Flow Rate (MVR) | 300°C/1.2 kg | ISO 1133 | 9.00 | cm3/10min |
| Outdoor applicability | UL 746C | f1 | ||
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.15 | % |
| Saturation, 23°C | ISO 62 | 0.35 | % | |
| melt mass-flow rate | 300°C/1.2 kg | ASTM D1238 | 10 | g/10 min |
| density | -- | ISO 1183 | 1.19 | g/cm³ |
| -- | ASTM D792 | 1.18 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | > 1.0E+15 | ohms | |
| Volume resistivity | IEC 60093 | > 1.0E+15 | ohms·cm | |
| Hot wire ignition | UL 746 | PLC 1 | ||
| High arc combustion index | UL 746 | PLC 0 | ||
| Compared to the anti leakage trace index | IEC 60112 | PLC 3 | ||
| UL 746 | PLC 3 | |||
| Dissipation factor | 60 Hz | IEC 60250 | 1.0E-3 | |
| 50 Hz | IEC 60250 | 1.0E-3 | ||
| 1 MHz | ASTM D150 | 8.5E-3 | ||
| 60 Hz | ASTM D150 | 2.4E-3 | ||
| 50 Hz | ASTM D150 | 2.4E-3 | ||
| Dielectric constant | 1 MHz | IEC 60250 | 2.70 | |
| 60 Hz | IEC 60250 | 2.60 | ||
| 50 Hz | IEC 60250 | 2.60 | ||
| 1 MHz | ASTM D150 | 2.90 | ||
| 50 kHz | ASTM D150 | 2.95 | ||
| 60 Hz | ASTM D150 | 2.95 | ||
| Dielectric strength | 3.20 mm, in Oil | IEC 60243-1 | 16 | KV/mm |
| 3.20 mm, in Oil | ASTM D149 | 17 | KV/mm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | H 358/30 | ISO 2039-1 | 90.0 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.