ASA Luran®S KR2863C BASF GERMANY
334
- Unit Price:US$ 2,480 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:30MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:High temperature resistance|UV resistance|high strength
- Application Areas:Fitness equipment|Automotive sector
- Color:--
- Grade:Impact resistant grade
Material Certification

TDS
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180/A | 60 kJ/m² |
-30°C | ISO 180/A | 10 kJ/m² | |
Charpy Notched Impact Strength | 23°C | ISO 179 | 60 kJ/m² |
-30°C | ISO 179 | 17 kJ/m² |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ISO 178 | 93.0 Mpa | |
Tensile strain | Yield,23°C | ISO 527-2 | 4.9 % |
tensile strength | Yield,23°C | ISO 527-2 | 62.0 Mpa |
Tensile modulus | ISO 527-2 | 2500 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
thermal conductivity | DIN 52612 | 0.17 W/m/K | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 7.0E-5到9.0E-5 cm/cm/°C |
Vicat softening temperature | -- | ISO 306/B50 | 130 °C |
-- | ISO 306/A50 | 140 °C | |
Hot deformation temperature | 0.45MPa,Annealed | ISO 75-2/B | 130 °C |
1.8MPa,Annealed | ISO 75-2/A | 109 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.16 % |
Saturation,23°C | ISO 62 | 0.60 % | |
Shrinkage rate | ISO 294-4 | 0.50-0.90 % | |
Melt Volume Flow Rate (MVR) | 260°C/5.0kg | ISO 1133 | 18.0 cm3/10min |
220°C/10.0kg | ISO 1133 | 7.00 cm3/10min | |
density | ISO 1183 | 1.16 g/cm³ |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Dissipation factor | 1MHz | IEC 60250 | 0.010 |
100Hz | IEC 60250 | 6E-03 | |
Dielectric constant | 100Hz | IEC 60250 | 3.10 |
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
Surface resistivity | IEC 60093 | 1E+14 ohms |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Ball Pressure Test | ISO 2039-1 | 110 Mpa |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
elongation | Break | ISO 527-3 | >50 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.