LCP SIVERAS™ L304M50 TORAY JAPAN
424
- Unit Price:US$ 5,070 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:enhance|Glass fiber reinforced|High toughness|High mobility
- Application Areas:Electrical components|Electrical appliances
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | (GF+MA)50 | |||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ASTM D790/ISO 178 | 170 | kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 17 | kg/cm²(MPa)[Lb/in²] | |
| elongation | ASTM D638/ISO 527 | 2.5 | % | |
| tensile strength | ASTM D638/ISO 527 | 135 | kg/cm²(MPa)[Lb/in²] | |
| Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 60 | kg·cm/cm(J/M)ft·lb/in | |
| Suspended wall beam without notch impact strength | ASTM D256 | 60 | J/m | |
| bending strength | ASTM D790 | 170 | Mpa | |
| Bending modulus | ASTM D790 | 17000 | Mpa | |
| elongation | Break | ASTM D1708 | 2.5 | % |
| tensile strength | ASTM D638 | 135 | Mpa | |
| Rockwell hardness | R -Sale | ASTM D785 | 105 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 1.3/1.5 | mm/mm.℃ | |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 265 | ℃(℉) |
| UL flame retardant rating | 0.380 mm | UL 94 | V-0 | |
| Linear coefficient of thermal expansion | Across Flow | ASTM D696 | 0.000015 | cm/cm/℃ |
| Flow | ASTM D696 | 0.000013 | cm/cm/℃ | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 265 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792/ISO 1183 | 1.82 | ||
| Water absorption rate | ASTM D570/ISO 62 | 0.01 | % | |
| 24 hr | ASTM D570 | 0.010 | % | |
| Shrinkage rate | TD | ASTM D955 | 0.29 | % |
| MD | ASTM D955 | 0.20 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Arc resistance | ASTM D495 | 190 | sec | |
| Dielectric constant | ASTM D150 | 4.50 | ||
| Dielectric strength | ASTM D149 | 50 | KV/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.