PA66 FL 66G30H1 BK DOMO CHEM GERMANY
327
- Unit Price:US$ 3,146 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:60MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Glass fiber reinforced|Thermal stability|enhance
- Application Areas:Automotive sector|Electronic field|Electrical field
- Color:--
- Grade:--
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 35 kJ/m² |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 30 kJ/m² |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Burning rate | FMVSS 302 | < 100 mm/min | |
UL flame retardant rating | 0.8 mm | UL 94 | HB |
ISO | ISO 1874 | PA6.M.14-080.GF30 |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 8500 Mpa | |
tensile strength | Break | ISO 527-2/5 | 130 Mpa |
Tensile strain | Break | ISO 527-2/5 | 2.5 % |
injection | Test Condition | Test Method | Test Result |
---|---|---|---|
drying temperature | 75 to 85 °C | ||
drying time | 2.0 to 4.0 hr | ||
Processing (melt) temperature | 270 to 290 °C | ||
Mold temperature | 90 to 110 °C |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 255 °C |
1.8 MPa, Unannealed | ISO 75-2/A | 245 °C | |
Vicat softening temperature | ISO 306/B50 | 250 °C | |
Melting temperature | ISO 11357-3 | 262 °C |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface resistivity | IEC 60093 | 1.0E+13 ohms | |
Volume resistivity | IEC 60093 | 1.0E+15 ohms·cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.