ABS Terluran® GP-35 INEOS STYRO KOREA
387
- Unit Price:US$ 1,800 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:66MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance|High mobility
- Application Areas:Electronic communication accessories|Household appliances
- Color:--
- Grade:High liquidity level
Technical Data Sheet
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Huangdu Index | DIN 6167 | 15 YI |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 90 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 22 kJ/m² |
-30°C | ISO 180/1A | 7 kJ/m² | |
Elongation at Break | 23°C | ISO 527-2 | 2.4 % |
Tensile modulus | 23°C | ISO 527-2 | 2300 Mpa |
bending strength | 23°C | ISO 178 | 65 Mpa |
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 19 kJ/m² |
-30°C | ISO 179/1eA | 7 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 130 kJ/m² |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 0.45MPaAnnealed | ISO 75-2/B | 95 °C |
1.80MPaAnnealed | ISO 75-2/A | 92 °C | |
Vicat softening temperature | ISO 306/A50 | 102 °C | |
ISO 306/B50 | 95 °C | ||
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 8E-05 cm/cm/°C |
TD | ISO 11359-2 | 1.1E-04 cm/cm/°C | |
导热系数 | DIN 52612 | 0.17 W/m/K |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | MD2.0mm | ISO 294-4 | 0.55 % |
Water absorption rate | (23°C,24hr) | ISO 62 | 0.95 % |
(23°C,50RH) | ISO 62 | 0.24 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+15 Ω.cm |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Ball Pressure Test | ISO 2039-1 | 99 Mpa |
flame retardant performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL -94 | HB 0.80mm | |
UL -94 | HB 1.50mm | ||
UL -94 | HB 3.00mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.