POM Delrin® 111DP DUPONT USA
187
- Unit Price:US$ 4,700 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:50MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Thermal stability|Fatigue resistance
- Application Areas:Engine parts|Home appliance components|Electronic and electrical components|Sports equipment
- Color:--
- Grade:--
Material Certification

Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 2.0 % | |
MediumDensity | 1.16 g/cm³ | ||
SpecificHeatCapacity of Melt | 3000 J/kg/°C | ||
melt mass-flow rate | ISO 1133 | 2.4 g/10min | |
Shrinkage rate | ISO 294-4 | 1.9 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | ISO 2039-2 | 94 | |
ISO 2039-2 | 122 |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB | |
IEC 60695-11-10,-20 | HB | ||
IEC 60695-11-10,-20 | HB | ||
FMVSS flammability | FMVSS302 | B | |
burning rate | ISO 3795 | 25 mm/min | |
UL flame retardant rating | UL 94 | HB |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Emission | VDA275 | <8.00 mg/kg |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 3150 Mpa | |
tensile strength | ISO 527-2 | 72.0 Mpa | |
Tensile strain | ISO 527-2 | 20 % | |
Nominal tensile fracture strain | ISO 527-2 | 40 % | |
Flexural modulus | ISO 178 | 2950 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | ISO 179/1eU | 340 kJ/m² | |
ISO 179/1eU | NoBreak |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/B | 165 °C | |
ISO 75-2/A | 98.0 °C | ||
melting temperature | ISO 11357-3 | 178 °C | |
AnnealingTemperature | 160 °C | ||
AnnealingTime-Optional | 30.0 min/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.