PP 9760 TOTAL EU
276
- Unit Price:US$ 1,547 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:12.5MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance|Creep resistance|High rigidity
- Application Areas:Toy
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 7.0 kJ/m² |
| -20°C | ISO 180 | 5.0 kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 8.0 kJ/m² |
| -20°C | ISO 179 | 5.5 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Bending modulus | ISO 178 | 1300 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 6.5 % |
| tensile strength | Yield | ISO 527-2 | 25.0 Mpa |
| Tensile modulus | ISO 527-2 | 1400 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melting temperature | ISO 3146 | 165 °C | |
| Vicat softening temperature | -- | ISO 306/B50 | 70.0 °C |
| -- | ISO 306/A50 | 140 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 48.0 °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 90.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 25 g/10min |
| Apparent density | ISO 1183 | 0.53 g/cm³ | |
| density | ISO 1183 | 0.905 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Scale | ISO 2039-2 | 83 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.