PA6 Grilon® BFZ3 EMS-CHEMIE SWITZERLAND
304
- Unit Price:US$ 3,359 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:46MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|Barrier resin|Food contact compliance
- Application Areas:Consumer goods sector|Electronic field|Electrical field|Industrial applications|chip|Pneumatic applications|Hydraulic applications|Pipe fittings|Wire and cable applications|container|Engineering accessories
- Color:--
- Grade:Blow molding grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -30℃-30°C | ISO 179/1eU | 无断裂 |
| Charpy Notched Impact Strength | 23℃23°C | ISO 179/1eA | 65 kJ/m² |
| -30℃-30°C | ISO 179/1eA | 15 kJ/m² | |
| Impact strength of simply supported beam without notch | 23℃23°C | ISO 179/1eU | 无断裂 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile strain | YieldYield | ISO 527-2 | 4 % |
| Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
| tensile strength | YieldYield | ISO 527-2 | 50 Mpa |
| Tensile modulus | ISO 527-2 | 1800 Mpa | |
| Ball Pressure Test | ISO 2039-1 | 95 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Linear coefficient of thermal expansion | TDTransverse | ISO 11359-2 | 0.00015 1/℃ |
| MDFlow | ISO 11359-2 | 0.00013 1/℃ | |
| Melting temperature | ISO 11357-3 | 222 °C | |
| Continuous use temperature | ---- 33 | Internal Method | 160 °C |
| ---- 22 | ISO 2578 | 80.0 to 110 °C | |
| Hot deformation temperature | 1.8 MPa,Unannealed264 psi, Unannealed | ISO 75-2/A | 50 °C |
| 0.45 MPa,Unannealed66 psi, Unannealed | ISO 75-2/B | 130 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | Equilibrium,23℃,50% RHEquilibrium, 73°F, 50% RH | ISO 62 | 3 % |
| Saturation,23℃Saturation, 73°F | ISO 62 | 9 % | |
| Shrinkage rate | MDFlow | ISO 294-4 | 1.1 % |
| TDAcross Flow | ISO 294-4 | 1.4 % | |
| density | ISO 1183 | 1.06 g/cm³ |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the anti leakage trace index | IEC 60112 | V | |
| Dielectric strength | IEC 60243-1 | 42 KV/mm | |
| Volume resistivity | IEC 60093 | 100000000000000 ohms·cm | |
| Surface resistivity | IEC 60093 | -- ohms |
| flame retardant performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Flammability level | UL 94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.