MVLDPE Daelim Poly® XP9200 Korea Daelim Basell
275
- Unit Price:US$ 1,880 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
gloss | 45°, 30.0 μm, Blown Film | ASTM D2457 | 87 |
turbidity | 30.0 μm, Blown Film | ASTM D1003 | 12 % |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tear strength | 横向Flow : 0.0300 mm | ASTM D1004 | 125 kN/m |
Flow : 0.0300 mm | ASTM D1004 | 122 kN/m |
squeeze out | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt Temperature | 150 to 190 °C |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Vicat softening temperature | ASTM D1525 | 106 °C | |
Melting temperature | ASTM D3418 | 116 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | 190°C/2.16 kg | ASTM D1238 | 1.5 g/10 min |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | MD : Break, 30 μm, Blown Film | ASTM D882 | 56.9 Mpa |
TD : Break, 30 μm, Blown Film | ASTM D882 | 45.1 Mpa | |
elongation | MD : Break, 30 μm, Blown Film | ASTM D882 | 580 % |
TD : Break, 30 μm, Blown Film | ASTM D882 | 620 % | |
Dart impact | 30 μm, Blown Film | ASTM D1709B | 670 g |
Initial sealing temperature | 30 μm, Blown Film | Internal Method | 95.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.