plas

LLDPE DOWLEX™  2036P DOW SPAIN

258
  • Unit Price:US$ 1,531 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    33MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Blow molding grade

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
gloss45°,25.4umASTM D-245790
turbidity25.4umASTM D-10032.6 %
gloss45°,25.4μmASTM D245790
turbidity25.4μmASTM D10032.6 %
Other performanceTest ConditionTest MethodTest Result
Thin film puncture strength25.4umInternal Method10.3 J/cm³
Film toughness25.4um,MDASTM D-882324 J/cm³
Film toughness25.4um,TDASTM D-882308 J/cm4
machinabilityTest ConditionTest MethodTest Result
Melt Temperature274 °C
Basic PerformanceTest ConditionTest MethodTest Result
densityASTM D-7920.935 g/m3
melt mass-flow rateASTM D-12382.5 g/10min
film thickness25.4 um
mechanical propertiesTest ConditionTest MethodTest Result
tensile strength25.4um,Yield,MDASTM D-88217.6 Mpa
tensile strength25.4um,Yield,MDASTM D-88216.9 Mpa
tensile strength25.4um,TD,BreakASTM D-88239.9 Mpa
tensile strength25.4um,MD,BreakASTM D-88259.2 Mpa
Elongation at Break25.4um,MDASTM D-882620 %
Elongation at Break25.4um,TDASTM D-882750 %
Dart impact25.4umASTM D-1709A57 g
Elmendorf tear strength25.4um,MDASTM D-192283 g
Elmendorf tear strength25.4um,TDASTM D-1922290 g
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureASTM D-1525119 °C
Melting temperatureInternal Method125 °C
Vicat softening temperatureASTM D1525119 °C
Melting temperatureInternal Method125 °C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate190°C/2.16kgASTM D12382.5 g/10min
filmTest ConditionTest MethodTest Result
elongationMD:Break,25μmASTM D882620 %
elongationTD:Break,25μmASTM D882750 %
Dart impact25μmASTM D1709A57 g
Elmendorf tear strengthMD:25μmASTM D192283 g
Elmendorf tear strengthTD:25μmASTM D1922290 g
film thickness25 µm
Thin film puncture strength25μmInternal Method10.3 J/cm³
Membrane strengthMD:25μmASTM D882324 J/cm³
Membrane strengthTD:25μmASTM D882308 J/cm³
tensile strengthMD:Yield,25μmASTM D88216.9 Mpa
tensile strengthTD:Yield,25μmASTM D88217.6 Mpa
tensile strengthMD:Break,25μmASTM D88259.2 Mpa
tensile strengthTD:Break,25μmASTM D88239.9 Mpa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.