Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 22.0 | J |
| Suspended wall beam without notch impact strength | 23°C | ASTM D4812 | 710 | J/m |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 50 | kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 13 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.600mm | UL 94 | V-0 | |
| 0.400mm | UL 94 | V-1 | ||
| 0.300mm | UL 94 | V-2 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Fracture, 50.0mm span | ASTM D790 | 131 | Mpa | |
| --6 | ISO 178 | 133 | Mpa | |
| --1 | ASTM D638 | 4400 | Mpa | |
| crack | ASTM D638 | 83.0 | Mpa | |
| ISO 527-2/5 | 82.0 | Mpa | ||
| ASTM D638 | 3.6 | % | ||
| ISO 527-2/5 | 3.6 | % | ||
| 50.0mm span | ASTM D790 | 4070 | Mpa | |
| --5 | ISO 178 | 4010 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:23to80°C | ISO 11359-2 | 3.4E-05 | cm/cm/°C |
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 117 | °C |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 121 | °C | |
| Linear coefficient of thermal expansion | TD:23to80°C | ISO 11359-2 | 7.7E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | 300°C/2.16kg | ISO 1133 | 27.0 | cm3/10min |
| Shrinkage rate | MD:24hr | ASTM D955 | 0.30-0.50 | % |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 13.0 | cm3/10min |
| melt mass-flow rate | 300°C/2.16kg | ASTM D1238 | 29 | g/10min |
| 300°C/1.2kg | ASTM D1238 | 14 | g/10min | |
| Shrinkage rate | TD:24hr | ASTM D955 | 0.30-0.50 | % |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.080 | % |
| Equilibrium,23°C,50%RH | ISO 62 | 0.040 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 10.0GHz | Internal Method | 6.9E-03 | |
| 5.00GHz | Internal Method | 6.9E-03 | ||
| 1.90GHz | Internal Method | 6.5E-03 | ||
| 1.10GHz | Internal Method | 6.7E-03 | ||
| Dielectric constant | 10.0GHz | Internal Method | 3.05 | |
| 5.00GHz | Internal Method | 3.06 | ||
| 1.90GHz | Internal Method | 3.06 | ||
| 1.10GHz | Internal Method | 3.07 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.