PPA Grivory® G 16 EMS-CHEMIE SWITZERLAND
238
- Unit Price:US$ 8,676 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High hardness|Chemical resistance
- Application Areas:Automotive Applications
- Color:--
- Grade:--
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| ISO Type | ISO 1874 | PA 6I/6T. FT. 09-030 | |
| gloss | 60° | ISO 2813 | 160 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 3000 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Glass transition temperature | ISO 11357-2 | 125 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 275°C/5.0 kg | ISO 1133 | 100 cm3/10min |
| Water absorption rate | Saturation, 23°C | ISO 62 | 7.0 % |
| Equilibrium, 23°C, 50% RH | ISO 62 | 2.0 % |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Carbon dioxide transmittance | 23°C3 | ASTM D256A | 40.0 cm³/m²/bar/24 hr |
| 23°C2 | ASTM D256A | 90.0 cm³/m²/bar/24 hr | |
| Oxygen permeability | 23°C3 | ASTM D256A | 10 cm³/m²/bar/24 hr |
| 23°C2 | ASTM D256A | 30 cm³/m²/bar/24 hr | |
| Water vapor permeability | 23°C, 85% RH | DIS 15106-1/-2 | 7.0 g/m²/24 hr |
| Tear resistance of pants type | TD | ISO 6383-1 | 5.00 N/mm |
| MD | ISO 6383-1 | 5.00 N/mm | |
| Elmendorf tear strength | TD | ISO 6383-2 | 10 N |
| MD | ISO 6383-2 | 10 N | |
| elongation | TD : Break | ISO 527-3 | 200 % |
| MD : Break | ISO 527-3 | 200 % | |
| TD : Yield | ISO 527-3 | 5.0 % | |
| MD : Yield | ISO 527-3 | 5.0 % | |
| tensile strength | MD : Break | ISO 527-3 | 80.0 Mpa |
| TD : Yield | ISO 527-3 | 85.0 Mpa | |
| MD : Yield | ISO 527-3 | 85.0 Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.