PP 3720E 10000 SABIC INNOVATIVE SHANGHAI
119
- Unit Price:US$ 857 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:2.23MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| melt mass-flow rate | 230℃,2.16kg | ISO 1133 | 18 | g/10min |
| density | ISO 1183 | 1.04 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 6 | KJ/m |
| Impact strength of simply supported beam without notch | -40℃ | ISO 179/1eU | 18 | KJ/m |
| Shore hardness | ISO 868 | 71 | ||
| tensile strength | Yield | ISO 527 | 28 | Mpa |
| Break | ISO 527 | 25 | Mpa | |
| elongation | Break | ISO 527 | 45 | % |
| Bending modulus | ASTM D-790 | 2200 | Mpa | |
| Impact strength of cantilever beam gap | 23℃ | ISO 180/4A | 6 | KJ/m |
| 0℃ | ISO 180/4A | 3.5 | KJ/m | |
| -20℃ | ISO 180/4A | 3 | KJ/m | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | 23℃-80℃ | ASTM D-696 | 110 | µm/mK |
| -30℃-30℃ | ASTM D-696 | 80 | µm/mK | |
| Hot deformation temperature | 0.45MPa | ISO 75/B | 110 | °C |
| Vicat softening temperature | 10N | ISO 306/A | 145 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 24 hours after injection moulding | SABIC method | 1.1 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.