PC TARFLON™ LEV1700 IDEMITSU JAPAN
222
- Unit Price:US$ 4,191 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20.8MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:heat-resisting
- Application Areas:Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| transmissivity | ISO 13468-1 | 90.0 % | |
| Refractive index | ASTM D542 | 1.585 |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 0.40mm | UL 94 | V-2 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield | ISO 527-2 | 65.0 Mpa |
| Nominal tensile fracture strain | ISO 527-2 | 95 % | |
| Bending modulus | ISO 178 | 2300 Mpa | |
| bending strength | ISO 178 | 90.0 Mpa | |
| Charpy Notched Impact Strength | ISO 179 | 40 kJ/m² | |
| bending strength | ISO 178 | 90 Mpa | |
| Bending modulus | ISO 178 | 2300 Mpa | |
| Elongation at Break | ISO 527-2 | 95 % | |
| tensile strength | Yield | ISO 527-2 | 65 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| RTI Str | UL 746 | 80.0 °C | |
| RTI Imp | UL 746 | 80.0 °C | |
| RTI Elec | UL 746 | 80.0 °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 6.5E-05 cm/cm/°C |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 129 °C |
| UL flame retardant rating | 0.400 mm | UL 94 | V-2 |
| Linear coefficient of thermal expansion | ISO 11359-2 | 0.000065 cm/cm/℃ | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 128 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | TD:2.00mm | Internal Method | 0.50-0.70 % |
| MD:2.00mm | Internal Method | 0.50-0.70 % | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.23 % |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 27.0 cm3/10min |
| Shrinkage rate | MD: 2.00 mm | Internal Method | 0.5-0.7 % |
| TD | Internal Method | 0.5-0.7 % | |
| Melt Volume Flow Rate (MVR) | MVR | ISO 1133 | 40 cm3/10min |
| Water absorption rate | Equilibrium,23℃, 50% RH | ISO 62 | 0.23 % |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Sale | ISO 2039-2 | 120 |
| M-Sale | ISO 2039-2 | 50 |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| ISO Shortcut | >PC< |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.