MBS Zylar® Zylar 631 INEOS STYRO KOREA
482
- Unit Price:US$ 3,316 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:180.1MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High temperature resistance|Chemical resistance|Aging resistance|thermal stability
- Application Areas:Sports equipment|Fitness equipment|Casters|Home appliance components|Electronic and electrical products|Toy
- Color:--
- Grade:Medical grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| turbidity | ISO 14782 | 1.5 % | |
| Transmittance rate | 3.2 mm | ASTM D1003 | 89 % |
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dart impact | ASTM D5420 | 11 J | |
| Charpy Notched Impact Strength | 23℃ | ISO 179 | 3.4 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | -- | ISO 178 | 57 Mpa |
| Bending modulus | -- | ISO 178 | 1890 Mpa |
| Tensile strain | Break,23℃ | ISO 527-2 | 36 % |
| tensile strength | Yield,23℃ | ISO 527-2 | 39 Mpa |
| Tensile modulus | 1 mm/min | ISO 527-2 | 2120 Mpa |
| Rockwell hardness | R-Scale | ISO 2039-2 | 70 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Maximum operating temperature | 250 °C | ||
| Vicat softening temperature | B50 | ISO 306 | 74 °C |
| Hot deformation temperature | 1.8 MPa,Annealed | ISO 75-2/A | 87 °C |
| 0.45 MPa,Annealed | ISO 75-2/B | 101 °C | |
| thermal conductivity | DIN 5261-1 | 0.17 W/m/K | |
| Linear coefficient of thermal expansion | ISO 11359 | 0.8-1.1 ×10-4/℃ |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | Saturation,23℃ | ISO 62 | 0.1 % |
| Melt Volume Flow Rate (MVR) | 200℃,5 kg | 5.8 cm3/10min | |
| density | ISO 1183 | 1.05 g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.