ASA/PC GELOY™ HRA150-BR8B018U SABIC INNOVATIVE US
637
- Unit Price:US$ 3,060 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:105MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High temperature resistance|UV resistance|Weather resistance
- Application Areas:Automotive sector|Outdoor applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 10 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 45 | kJ/m² |
| -30°C | ISO 180/1A | 10 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 65 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 20 | % | |
| Burning wire flammability index | 3.20mm | IEC 60695-2-12 | 750 | °C |
| UL flame retardant rating | 3.00mm | UL 94 | HB | |
| 0.750mm | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Taber abraser | 1000Cycles,1000g,CS-17Wheel | Internal Method | 125 | mg |
| bending strength | ISO 178 | 80.0 | Mpa | |
| Bending modulus | ISO 178 | 2400 | Mpa | |
| crack | ISO 527-2/50 | >50 | % | |
| ISO 527-2/5 | 120 | % | ||
| yield | ISO 527-2/5 | 4.0 | % | |
| crack | ISO 527-2/50 | 59.0 | Mpa | |
| ISO 527-2/5 | 55.0 | Mpa | ||
| yield | ISO 527-2/50 | 59.0 | Mpa | |
| Tensile modulus | ISO 527-2/1 | 2500 | Mpa | |
| yield | ISO 527-2/5 | 55.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C |
| Ball Pressure Test | 105°C7 | IEC 60695-10-2 | Pass | |
| 75°C | IEC 60695-10-2 | Pass | ||
| 1.8MPa, unannealed, 100mm span | ISO 75-2/Ae | 101 | °C | |
| 0.45MPa, unannealed, 100mm span | ISO 75-2/Be | 125 | °C | |
| thermal conductivity | ISO 8302 | 0.20 | W/m/K | |
| RTI Elec | UL 746 | 50.0 | °C | |
| RTI Imp | UL 746 | 50.0 | °C | |
| RTI | UL 746 | 50.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.60 | % |
| Equilibrium,23°C,50%RH | ISO 62 | 0.20 | % | |
| Shrinkage rate | MD1 | Internal Method | 0.40-0.60 | % |
| Melt Volume Flow Rate (MVR) | 260°C/5.0kg | ISO 1133 | 15.0 | cm3/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | >1.0E+15 | ohms | |
| Volume resistivity | IEC 60093 | >1.0E+15 | ohms·cm | |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 17 | KV/mm |
| Relative permittivity | 1MHz | IEC 60250 | 2.90 | |
| Dissipation factor | 1MHz | IEC 60250 | 0.015 | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 3 | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Sale | ISO 2039-2 | 118 | |
| Ball Pressure Test | H358/30 | ISO 2039-1 | 104 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.