Material Description
- Material Properties:Flame retardant|Glass fiber reinforced|High temperature resistance|Filler: Glass fiber reinforced material|40% filler by weight
- Application Areas:sporting goods|Automotive Applications|Electrical applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 45 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 0.200mm | UL 94 | V-0 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Friction coefficient | 0.25 | ||
| shear strength | 23°C | JISK7214 | 75.0 Mpa |
| bending strength | 23°C | ISO 178 | 290 Mpa |
| Bending modulus | 23°C | ISO 178 | 15000 Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 1.7 % |
| tensile strength | Yield,23°C | ISO 527-2 | 190 Mpa |
| Taber abraser | 1000Cycles | ISO 9352 | 50.0 mg |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 3.5E-05 cm/cm/°C |
| MD | ISO 11359-2 | 2.3E-05 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 278 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 260 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | 23°C,24hr | ISO 62 | 0.020 % |
| Shrinkage rate | MD:3.00mm4 | Internal Method | 0.20 % |
| TD:3.00mm2 | Internal Method | 0.80 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dissipation factor | 23°C,1MHz | IEC 60250 | 2E-03 |
| Dielectric constant | 23°C,1MHz | IEC 60250 | 3.60 |
| Dielectric strength | IEC 60243-1 | 25 KV/mm | |
| Volume resistivity | IEC 60093 | 1E+16 ohms·cm |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Scale | ISO 2039-2 | 122 |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| BarFlowLength | 320°C,1.00mm | Internal Method | 165 mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.