Material Description
- Material Properties:Thermal stability|High temperature resistance
- Application Areas:Automotive components|glasses|lens|lens
- Color:--
- Grade:Optical grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| turbidity | 2540μm | ASTM D1003 | 0.40 | % |
| transmissivity | 2540μm | ASTM D1003 | 87.0 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Suspended wall beam without notch impact strength | -30°C | ASTM D4812 | 无断裂 | |
| 23°C | ASTM D4812 | 无断裂 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ASTM D638 | 2310 | Mpa | |
| tensile strength | Yield | ASTM D638 | 64.0 | Mpa |
| bending strength | Yield,50.0mmSpan4 | ASTM D790 | 96.0 | Mpa |
| --5,6 | ISO 178 | 97.0 | Mpa | |
| Bending modulus | 50.0mmSpan | ASTM D790 | 2310 | Mpa |
| elongation | Break | ASTM D638 | 78 | % |
| Yield | ASTM D638 | 6.0 | % | |
| tensile strength | Break | ASTM D638 | 60.0 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 129 | °C |
| Vicat softening temperature | ASTM D15257 | 145 | °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | 通过 | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ISO 11359-2 | 6.1E-05 | cm/cm/°C |
| TD:-40to40°C | ISO 11359-2 | 6.2E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 8.00 | cm3/10min |
| Shrinkage rate | MD | Internal Method | 0.77 | % |
| TD | Internal Method | 0.77 | % | |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.14 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 1.10GHz | Internal Method | 2.80 | |
| Dissipation factor | 1.10GHz | Internal Method | 6.3E-03 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.