PC LPC1001F BK LUCK ENPLA KOREA
276
- Unit Price:US$ 2,419 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Impact resistant grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Suspended wall beam without notch impact strength | 3.18 mm | ASTM D256 | 590 J/m |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 0.8 mm | UL 94 | V-0 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | ASTM D790 | 82.4 Mpa | |
| Bending modulus | ASTM D790 | 2280 Mpa | |
| tensile strength | ASTM D638 | 53.0 Mpa |
| injection | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Screw speed | 30 to 50 rpm | ||
| Back pressure | 0.490 to 2.94 Mpa | ||
| Mold temperature | 50 to 80 °C | ||
| Spray nozzle temperature | 295 to 315 °C | ||
| Temperature at the front of the material cylinder | 285 to 305 °C | ||
| Temperature in the middle of the barrel | 280 to 300 °C | ||
| Temperature at the rear of the barrel | 270 to 290 °C | ||
| drying time | 3.0 to 5.0 hr | ||
| drying temperature | 100 to 110 °C |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 122 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 260°C/5.0 kg | ASTM D1238 | 22 g/10 min |
| Shrinkage rate | Flow | ASTM D955 | 0.60 - 0.65 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.