plas

PC LEXAN™  123R-111 SABIC INNOVATIVE NANSHA

537
  • Unit Price:US$ 1,878 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    182MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
transmissivity2540 μmASTM D100388.0 %
turbidity2540 μmASTM D10031.0 %
Refractive indexASTM D5421.586
impact performanceTest ConditionTest MethodTest Result
Dart impact23°CASTM D3029169 J
Suspended wall beam without notch impact strength23°CASTM D48123200 J/m
Impact strength of cantilever beam gapASTM D1822546 kJ/m²
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating0.76 mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest Result
bending strengthYield, 50.0 mm SpanASTM D79093.0 Mpa
Bending modulus50.0 mm SpanASTM D7902340 Mpa
Taber abraser1000 Cycles, 1000 g, CS-17 WheelASTM D104410.0 mg
elongationBreakASTM D638110 %
elongationYieldASTM D6387.0 %
tensile strengthBreakASTM D63865.0 Mpa
tensile strengthYieldASTM D63862.0 Mpa
injectionTest ConditionTest MethodTest Result
drying temperature120 °C
drying time3.0 to 4.0 hr
Suggested maximum moisture content0.020 %
Suggested injection volume40 to 60 %
Temperature at the rear of the barrel260 to 280 °C
Temperature in the middle of the barrel270 to 295 °C
Temperature at the front of the material cylinder280 to 305 °C
Spray nozzle temperature275 to 300 °C
Processing (melt) temperature280 to 305 °C
Mold temperature70 to 95 °C
Back pressure0.300 to 0.700 Mpa
Screw speed40 to 70 rpm
Exhaust hole depth0.025 to 0.076 mm
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8 MPa, Unannealed, 6.40 mmASTM D648132 °C
Hot deformation temperature0.45 MPa, Unannealed, 6.40 mmASTM D648137 °C
specific heatASTM C3511260 J/kg/°C
Linear coefficient of thermal expansion-40 to 95°C,FlowASTM E8316.8E-5 cm/cm/°C
Vicat softening temperatureASTM D15255154 °C
RTIUL 746130 °C
RTI ImpUL 746130 °C
RTI ElecUL 746130 °C
thermal conductivityASTM C1770.19 W/m/K
Physical propertiesTest ConditionTest MethodTest Result
Specific volumeASTM D7920.830 cm³/g
melt mass-flow rate300°C/1.2 kgASTM D123818 g/10 min
Outdoor applicabilityUL 746Cf1
Water absorption rateEquilibrium, 23°CASTM D5700.35 %
Shrinkage rate3.20 mm,FlowInternal Method0.50 - 0.70 %
Water absorption rateEquilibrium, 100°CASTM D5700.58 %
Water absorption rate24 hrASTM D5700.15 %
Electrical performanceTest ConditionTest MethodTest Result
Hot wire ignitionUL 746PLC 4
Dissipation factor1 MHzASTM D1500.010
Dissipation factor60 HzASTM D1509.0E-4
Dissipation factor50 HzASTM D1509.0E-4
Dielectric constant1 MHzASTM D1502.96
Dielectric constant50 kHzASTM D1503.17
Dielectric constant60 HzASTM D1503.17
Dielectric strength3.20 mm, in AirASTM D14915 KV/mm
High voltage arc tracing rateUL 746PLC 2
High arc combustion indexUL 746PLC 1
Compared to the anti leakage trace indexUL 746PLC 2
Volume resistivityASTM D257> 1.0E+17 ohms·cm
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTM D785118
Rockwell hardnessM-ScaleASTM D78570
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.