PA66 AKROMID®  A3 GF 25 1 BK AKRO-PLASTIC GERMANY

325
  • Unit Price:US$ 2,852 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    30MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:enhanceThermal stabilityFiller: Glass fiber reinforced material25% filler by weight
  • Application Areas:Industrial applicationsAutomotive sectorengineering application
  • Color:--
  • Grade:--

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest Result
spiral flow length内部方法89.0 CM
Shrinkage rateISO 294-41.3 %
Shrinkage rateISO 294-40.20 %
Water absorption rateISO 625.7to6.3 %
moisture absorptionISO 11102.0to2.2 %
hardnessTest ConditionTest MethodTest Result
ball-indentation hardnessISO 2039-1225 Mpa
flammabilityTest ConditionTest MethodTest Result
burning rateFMVSS302<100 mm/min
UL flame retardant ratingUL 94HB
Burning wire flammability indexIEC 60695-2-12650 °C
Supplementary InformationTest ConditionTest MethodTest Result
ReinforcementContentISO 117225 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/18500 Mpa
tensile strength ISO 527-2/5185 Mpa
Tensile strainISO 527-2/53.6 %
Flexural modulusISO 1787600 Mpa
bending strengthISO 178260 Mpa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of simply supported beam without notchISO 179/1eU64 kJ/m²
Impact strength of simply supported beam without notchISO 179/1eU70 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityIEC 600931E+12 ohms
Volume resistivityIEC 600931E+13 ohms·cm
Compared to the Leakage Tracking Index (CTI)IEC 60112 V
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/B260 °C
Heat distortion temperatureISO 75-2/A255 °C
melting temperatureDIN EN11357-1262 °C
TemperatureIndexIEC 216130to150 °C
TemperatureIndexIEC 216160to175 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.