plas

PA66 LNP™ LUBRICOMP™  RL-4540 BK SABIC INNOVATIVE US

215
  • Unit Price:US$ 5,559 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    48.5MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Thermal stabilitywear resistant
  • Application Areas:Automotive External PartsElectronic and Electrical Applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 180/1A5.2 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U88 kJ/m²
Dart impact23°C,TotalEnergyASTM D37636.70 J
Multi axis Instrumented Impact EnergyISO 6603-21.20 J
mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthBreakASTM D63861.0 Mpa
tensile strengthBreakISO 527-2/563.0 Mpa
elongationYieldASTM D63822 %
Tensile strainYieldISO 527-2/526 %
elongationBreakASTM D63823 %
Tensile strainBreakISO 527-2/527 %
Bending modulus50.0mmSpanASTM D7902260 Mpa
Bending modulusISO 1782400 Mpa
Friction coefficientDynamicASTM D3702Modified0.020
Friction coefficientStaticASTM D3702Modified0.045
Wear factorWasherASTM D3702Modified3.50 10^-10in^5-min/ft-lb-hr
Tensile modulusASTM D6382620 Mpa
Tensile modulusISO 527-2/12730 Mpa
tensile strengthYieldASTM D63861.0 Mpa
tensile strengthYieldISO 527-2/563.0 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO 75-2/Af63.0 °C
Linear coefficient of thermal expansionMD:-30to30°CASTM D6968.4E-05 cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTM D6969.4E-05 cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648237 °C
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpanISO 75-2/Bf200 °C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64864.0 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateMD:24hrASTM D9551.0-3.0 %
Shrinkage rateTD:24hrASTM D9551.0-3.0 %
Water absorption rate24hr,50%RHASTM D5700.84 %
Water absorption rateEquilibrium,23°C,50%RHISO 621.1 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.