PC LEXAN™ ML6413 SABIC INNOVATIVE US
73
- Unit Price:US$ 4,580 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:14MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility|High optical masking
- Application Areas:Lighting applications|Electronic and Electrical Applications|Plastic bag|currency
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 72.0 | J |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 60 | kJ/m² |
| -30°C | ISO 180/1A | 15 | kJ/m² | |
| 23°C | ASTM D256 | 790 | J/m | |
| -30°C | ASTM D256 | 150 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Burning wire flammability index | 1.6mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 3.0mm | UL 94 | 5VA | |
| 2.0mm | UL 94 | 5VB | ||
| 1.6mm | UL 94 | V-0 | ||
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 800 | °C |
| 3.0mm | IEC 60695-2-13 | 800 | °C | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | Yield,50.0mmSpan | ASTM D790 | 85.0 | Mpa |
| ISO 178 | 90.0 | Mpa | ||
| Bending modulus | ISO 178 | 2350 | Mpa | |
| 50.0mmSpan | ASTM D790 | 2250 | Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 100 | % |
| elongation | Break | ASTM D638 | 100 | % |
| Tensile modulus | ASTM D638 | 2500 | Mpa | |
| ISO 527-2/1 | 2350 | Mpa | ||
| tensile strength | Yield | ASTM D638 | 58.0 | Mpa |
| Yield | ISO 527-2/50 | 62.0 | Mpa | |
| Break | ASTM D638 | 55.0 | Mpa | |
| Break | ISO 527-2/50 | 58.0 | Mpa | |
| elongation | Yield | ASTM D638 | 5.0 | % |
| Tensile strain | Yield | ISO 527-2/50 | 5.0 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | -- | ISO 306/B50 | 134 | °C |
| ASTM D15259 | 134 | °C | ||
| RTI Str | UL 746 | 100 | °C | |
| RTI Imp | UL 746 | 100 | °C | |
| RTI Elec | UL 746 | 100 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 118 | °C |
| 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 125 | °C | |
| 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 115 | °C | |
| Vicat softening temperature | -- | ISO 306/B120 | 135 | °C |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.7E-05 | cm/cm/°C |
| MD:-40to40°C | ISO 11359-2 | 7E-05 | cm/cm/°C | |
| TD:-40to40°C | ASTME831 | 5.9E-05 | cm/cm/°C | |
| TD:-40to40°C | ISO 11359-2 | 7E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.20 | g/cm³ | |
| ISO 1183 | 1.20 | g/cm³ | ||
| melt mass-flow rate | 260°C/5.0kg | ASTM D1238 | 24 | g/10min |
| Melt Volume Flow Rate (MVR) | 260°C/5.0kg | ISO 1133 | 20.0 | cm3/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.40-0.80 | % |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.30 | % |
| Equilibrium,23°C,50%RH | ISO 62 | 0.10 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot wire ignition | HWI | UL 746 | PLC 3 | |
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 2 | |
| Volume resistivity | ASTM D257 | >1.0E+15 | ohms·cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.