Material Properties:Low viscosity|Flame retardant|transparent
Application Areas:Profile|building materials
Color:--
Grade:Injection grade
Technical Data Sheet
optical performance
Test Condition
Test Method
Test Result
Refractive index
ASTM D542
1.586
transmissivity
2540 μm
ASTM D1003
88.0 %
turbidity
2540 μm
ASTM D1003
1.0 %
impact performance
Test Condition
Test Method
Test Result
Impact strength of cantilever beam gap
ASTM D1822
546 kJ/m²
Dart impact
23°C
ASTM D3029
169 J
Dart impact
23°C, Energy at Peak
ASTM D3763
62.0 J
Suspended wall beam without notch impact strength
23°C5
ISO 180/1U
无断裂
Suspended wall beam without notch impact strength
-30°C5
ISO 180/1U
无断裂
Suspended wall beam without notch impact strength
23°C
ASTM D4812
3200 J/m
Impact strength of simply supported beam without notch
23°C
ISO 179/1eU
无断裂
Impact strength of simply supported beam without notch
-30°C
ISO 179/1eU
无断裂
Charpy Notched Impact Strength
23°C
ISO 179/1eA
65 kJ/m²
Charpy Notched Impact Strength
-30°C
ISO 179/1eA
12 kJ/m²
flammability
Test Condition
Test Method
Test Result
UL flame retardant rating
0.71 mm
UL 94
HB
Radiation board grade
UL Unspecified
TRUE
mechanical properties
Test Condition
Test Method
Test Result
Taber abraser
1000 Cycles, 1000 g, CS-17 Wheel
ASTM D1044
10.0 mg
bending strength
Yield, 50.0 mm Span
ASTM D790
96.0 Mpa
Bending modulus
50.0 mm Span
ASTM D790
2340 Mpa
elongation
Break
ASTM D638
130 %
elongation
Yield
ASTM D638
7.0 %
tensile strength
Break
ASTM D638
68.0 Mpa
tensile strength
Yield
ASTM D638
62.0 Mpa
injection
Test Condition
Test Method
Test Result
drying time
3.0 to 4.0 hr
drying temperature
120 °C
Suggested maximum moisture content
0.020 %
Suggested injection volume
40 to 60 %
Temperature at the rear of the barrel
260 to 280 °C
Temperature in the middle of the barrel
270 to 295 °C
Temperature at the front of the material cylinder
280 to 305 °C
Spray nozzle temperature
275 to 300 °C
Processing (melt) temperature
280 to 305 °C
Mold temperature
70 to 95 °C
Back pressure
0.300 to 0.700 Mpa
Screw speed
40 to 70 rpm
Exhaust hole depth
0.025 to 0.076 mm
thermal performance
Test Condition
Test Method
Test Result
Hot deformation temperature
1.8 MPa, Unannealed, 6.40 mm
ASTM D648
129 °C
Hot deformation temperature
0.45 MPa, Unannealed, 6.40 mm
ASTM D648
137 °C
Vicat softening temperature
ASTM D15257
154 °C
Linear coefficient of thermal expansion
-40 to 95°C,Flow
ASTM E831
6.8E-5 cm/cm/°C
specific heat
ASTM C351
1250 J/kg/°C
thermal conductivity
ASTM C177
0.25 W/m/K
RTI Elec
UL 746
130 °C
RTI Imp
UL 746
130 °C
RTI
UL 746
130 °C
Physical properties
Test Condition
Test Method
Test Result
Specific volume
ASTM D792
0.830 cm³/g
melt mass-flow rate
300°C/1.2 kg
ASTM D1238
18 g/10 min
Shrinkage rate
3.20 mm,Flow
Internal Method
0.50 - 0.70 %
Outdoor applicability
UL 746C
f2
Water absorption rate
Equilibrium, 100°C
ASTM D570
0.58 %
Water absorption rate
Equilibrium, 23°C
ASTM D570
0.35 %
Water absorption rate
24 hr
ASTM D570
0.15 %
Electrical performance
Test Condition
Test Method
Test Result
Volume resistivity
ASTM D257
> 1.0E+17 ohms·cm
Dielectric strength
3.20 mm, in Air
ASTM D149
15 KV/mm
Dielectric constant
60 Hz
ASTM D150
3.17
Dielectric constant
50 kHz
ASTM D150
3.17
Dielectric constant
1 MHz
ASTM D150
2.96
Dissipation factor
50 Hz
ASTM D150
9.0E-4
Dissipation factor
60 Hz
ASTM D150
9.0E-4
Dissipation factor
1 MHz
ASTM D150
0.010
Compared to the anti leakage trace index
UL 746
PLC 2
High arc combustion index
UL 746
PLC 1
High voltage arc tracing rate
UL 746
PLC 2
Hot wire ignition
UL 746
PLC 2
hardness
Test Condition
Test Method
Test Result
Rockwell hardness
R-Scale
ASTM D785
118
Rockwell hardness
M-Scale
ASTM D785
70
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.