plas

TPEE Hytrel®  3548 DUPONT USA

339
  • Unit Price:US$ 6,553 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    19MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:UV resistanceThermal stability
  • Application Areas:Automotive ApplicationsElectrical applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

flammabilityTest ConditionTest MethodTest Result
FMVSS flammabilityFMVSS302B
UL flame retardant rating3.0mmIEC 60695-11-10,-20HB
UL flame retardant rating1.5mmIEC 60695-11-10,-20HB
UL flame retardant rating3.0mmUL 94HB
UL flame retardant rating1.5mmUL 94HB
Burning rate1.00mmISO 3795<100 mm/min
elastomerTest ConditionTest MethodTest Result
tear strengthFlowISO 34-160 kN/m
tear strength横向FlowISO 34-180 kN/m
mechanical propertiesTest ConditionTest MethodTest Result
Bending modulusISO 17825.0 Mpa
Nominal tensile fracture strainISO 527-2200 %
Tensile strainBreakISO 527-2190 %
tensile strength50%StrainISO 527-26.00 Mpa
tensile strength10%StrainISO 527-22.50 Mpa
tensile strength5.0%StrainISO 527-21.50 Mpa
tensile strengthBreakISO 527-210.0 Mpa
Tensile modulusISO 527-225.0 Mpa
thermal performanceTest ConditionTest MethodTest Result
Melting temperatureISO 11357-3157 °C
Physical propertiesTest ConditionTest MethodTest Result
Water absorption rateEquilibrium,23°C,2.00mm,50%RHISO 620.80 %
Water absorption rateSaturation,23°C,2.00mmISO 6212 %
Water absorption rate23°C,24hrISO 626.9 %
Shrinkage rateMDISO 294-40.80 %
Shrinkage rateTDISO 294-40.80 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreD,15SecISO 86824
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.